[article]
| Titre : |
Improved wear resistance of dendrite composite eutectic Fe-B alloy |
| Type de document : |
texte imprimé |
| Auteurs : |
Licai Fu, Auteur ; Jun Yang, Auteur ; Qinling Bi, Auteur |
| Année de publication : |
2012 |
| Article en page(s) : |
05 p. |
| Note générale : |
Tribology |
| Langues : |
Anglais (eng) |
| Mots-clés : |
Dendrites Eutectic alloys Friction Oxidation Wear resistance |
| Index. décimale : |
621.5 Energie pneumatique. Machinerie et outils. Réfrigération |
| Résumé : |
The dry-sliding tribological properties of the dendrite composite eutectic Fe-B alloys (Fe94.3B5.7, Fe75B25 Fe67B33) were studied comparatively with various sliding speeds. The friction coefficient of the Fe-B alloy changes slightly with the boron content. The wear rate of the Fe94.3B5.7 alloy with about 30 vol. % dendrite t-Fe2B is only one third of Fe75B25 alloy with 15 vol. % dendrite and Fe67B33 alloy with 90 vol. % dendrite in the high sliding speed. First, a hard t-Fe2B phase reduced the wear of the Fe-B alloy directly. Second, the compactly oxide layers resulting from oxidation of the alpha-Fe on the worn surfaces also decreases the wear rate of Fe-B alloys. On the whole, the wear rate of the Fe94.3B5.7 is lower than Fe67B33 and Fe75B25. |
| DEWEY : |
621.5 |
| ISSN : |
0742-4787 |
| En ligne : |
http://scitation.aip.org/getabs/servlet/GetabsServlet?prog=normal&id=JOTRE900013 [...] |
in Transactions of the ASME . Journal of tribology > Vol. 133 N° 4 (Octobre 2011) . - 05 p.
[article] Improved wear resistance of dendrite composite eutectic Fe-B alloy [texte imprimé] / Licai Fu, Auteur ; Jun Yang, Auteur ; Qinling Bi, Auteur . - 2012 . - 05 p. Tribology Langues : Anglais ( eng) in Transactions of the ASME . Journal of tribology > Vol. 133 N° 4 (Octobre 2011) . - 05 p.
| Mots-clés : |
Dendrites Eutectic alloys Friction Oxidation Wear resistance |
| Index. décimale : |
621.5 Energie pneumatique. Machinerie et outils. Réfrigération |
| Résumé : |
The dry-sliding tribological properties of the dendrite composite eutectic Fe-B alloys (Fe94.3B5.7, Fe75B25 Fe67B33) were studied comparatively with various sliding speeds. The friction coefficient of the Fe-B alloy changes slightly with the boron content. The wear rate of the Fe94.3B5.7 alloy with about 30 vol. % dendrite t-Fe2B is only one third of Fe75B25 alloy with 15 vol. % dendrite and Fe67B33 alloy with 90 vol. % dendrite in the high sliding speed. First, a hard t-Fe2B phase reduced the wear of the Fe-B alloy directly. Second, the compactly oxide layers resulting from oxidation of the alpha-Fe on the worn surfaces also decreases the wear rate of Fe-B alloys. On the whole, the wear rate of the Fe94.3B5.7 is lower than Fe67B33 and Fe75B25. |